KANEVINYL T5HX

Technical Data Sheet

Kanevinyl T5HX

 

Item

Kanevinyl

T5HX

Method

Vinyl Chrolide

content ( % )

82

 

Vinyl Acetate

content ( % )

10

Kaneka Method

( FT- IR )

Hydroxyl Group

content ( % )

8

Kaneka Method

( modified JIS K0070 )

K Value ( - )

51

ISO 1269 ,

JIS K7367-2

Tg ( ℃ )

69

KANEKA method

( DSC )

Solution

viscosity ( cps )

 

Type B viscometer

Fomula 1  *

80

measured at 25℃,

dissolved at 30℃×20 min

Fomula 2  *

300

measured at 25℃,

dissolved at 30℃×20 min

 

* Fomula 1; Resin/MEK=20/80

  Fomula 2; Resin/EAC=20/80

 

This is only reference figures, not guaranteed ones

Above data and information are based on our reliable test.

凹版油墨、木工涂料、加工油墨