Clear Coating based on Lac 4501
Pos. |
Ingredient |
Weight % |
Incorporation Method |
1 |
Lac 4501 |
80 |
add |
2 |
BYK-7420 ES |
0.2 |
1500rpmAdd under stirring |
3 |
BYK-028 |
0.8 |
addunder stirring for 10 mim/1500rpm |
4 |
DPnB |
3.20 |
mixingboth then add under stirring for 5 mim/1500rpm |
5 |
DPM |
3.20 |
|
6 |
water |
7.00 |
7 |
BYK-349 |
0.4 |
Addunder stirring |
8 |
Aquacer-539 |
2 |
9 |
H600vf(50%with DPM) |
0.8 |
Addunder stirring for adjusting viscosity |
10 |
water |
2.2 |
100 |
水性木器参考配方