Clear Coating based on XK-258

Pos.

Ingredient

Weight %

Incorporation Method


1

XK-258

80

add

2

L-RDS(10%, D.W.)

5

Addunder stirring


3

BYK-022

0.4

 

2000rpm/20min

4

BYK-028

0.8


5

DPnB

3.2

mixingboth then add under stirring for 5 mim/1500rpm

6

DPM

2.1

7

water

5


8

BYK-347

0.5

Addunder stirring for 5min/1000rpm


9

BYK-425(20%,D.W.)

2

Addunder stirring for 5min/1000rpm

10

water

1


   

100

 

 

应用:水性木器无气喷涂工艺